Polyurea-Based Coatings

By
Dudley J. Primeaux, II
Dudley J. Primeaux, II
VersaFlex Inc.
Search for other works by this author on:
Published:
2015
Page range:
118 - 131
Publication history
December 26, 2014

Abstract

Two-component polyurea elastomeric coating/lining systems are the newest technology in the protective coating/lining industry and a wide variety of applications have been developed. These include coating/lining applications over concrete, geotextile membranes, various metals for corrosion and decorative areas, and some plastics. This article discusses the formulation basics of polyurea technology and compares the technology to that of polyurethane and polyurethane/polyurea systems. It addresses performance issues and describes application processing considerations and safety practices of polyurea coating/lining systems.

You do not currently have access to this content.
Don't already have an account? Register

Dudley J. Primeaux, II, 2015. "Polyurea-Based Coatings", Protective Organic Coatings, Kenneth B. Tator

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal