Polyester and Vinyl Ester Coatings

By
Kenneth B. Tator
Kenneth B. Tator
KTA-Tator, Inc.
Search for other works by this author on:
William R. Slama
William R. Slama
AkzoNobel
Search for other works by this author on:
Published:
2015
Page range:
100 - 110
Publication history
December 26, 2014

Abstract

This article provides a discussion on polyester coating applications such as powder coatings, can coatings, and automotive paints. It includes an overview, structure, properties, and benefits of vinyl ester resins. The article discusses the additives for both unsaturated polyester and vinyl ester coatings, namely, curing systems, thixotropic agents and fillers. It exemplifies polyester and vinyl ester coating, lining and flooring systems that are used for top-to-bottom protection of industrial plants and equipment. The article also highlights the concerns to be addressed when using polyesters and vinyl esters.

You do not currently have access to this content.
Don't already have an account? Register

Kenneth B. Tator, William R. Slama, 2015. "Polyester and Vinyl Ester Coatings", Protective Organic Coatings, Kenneth B. Tator

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal