Polyaspartic Coatings

By
Edward P. Squiller
Edward P. Squiller
Bayer MaterialScience LLC
Search for other works by this author on:
Steven Reinstadtler
Steven Reinstadtler
Bayer MaterialScience LLC
Search for other works by this author on:
Published:
2015
Page range:
132 - 138
Publication history
December 26, 2014

Abstract

Polyaspartic coating technology has found utility in a variety of coating applications, including corrosion protection and flooring topcoats, as these coatings are based on aliphatic polyisocyanates and aliphatic diamines. This article describes the chemistry of polyaspartic esters and curing characteristics and performance properties of polyaspartic coatings. It also provides information on curing corrosion protection coating systems, polyaspartic floor coatings, and safe-use recommendations for handling isocyanates.

You do not currently have access to this content.
Don't already have an account? Register

Edward P. Squiller, Steven Reinstadtler, 2015. "Polyaspartic Coatings", Protective Organic Coatings, Kenneth B. Tator

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal