Book Chapter

Polysiloxane Hybrid Coatings

By
Gerald L. Witucki
Gerald L. Witucki
Dow Corning Corporation
Search for other works by this author on:
Published:
2015
Page range:
185 - 188
Publication history
December 26, 2014

Abstract

This article focuses on technologies in the protective coatings field, namely, polysiloxane hybrids and related materials. Industrial maintenance topcoats, including silicone alkyds, silicone epoxies, and polysiloxanes are reviewed. The article discusses two major application areas of protective coatings, namely, architectural coatings and automotive clear coats.

You do not currently have access to this content.
Don't already have an account? Register

Gerald L. Witucki, 2015. "Polysiloxane Hybrid Coatings", Protective Organic Coatings, Kenneth B. Tator