A major effort in the development of thermal spray applications has been the improvement of process reliability and predictability in response to process changes. The ability to model a process is a prerequisite to understanding and controlling it. This article provides an overview of thermal spray process modeling, as it applies to the engineering of new thermal spray equipment and coating development.

You do not currently have access to this content.
Don't already have an account? Register

2013. "Process Modeling", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal