Abstract

This article begins with a description of the advantages and disadvantages of thermal spraying. It provides a discussion on the importance of substrate processing prior to coating and the role of undercutting in repair. The article reviews the steps for substrate preparation, namely, cleaning, roughening, masking, and preheating. Information on the equipment and process variables of dry abrasive grit blasting are also provided. The article describes the roles of spray stream and the spray pattern for all thermal spray processes. It discusses the defects arising from poor temperature control and from the variables influencing the manipulation of the spray torch. The article concludes with helpful information on calculating the process efficiency of thermal spraying.

You do not currently have access to this content.
Don't already have an account? Register

2013. "Introduction to Coating Design and Processing", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal