Skip to Main Content
ASM Handbook

Thermal Spray Technology

Edited by
Robert C. Tucker, Jr.
Robert C. Tucker, Jr.
The Tucker Group
Search for other works by this author on:
ASM International
Volume
5A
ISBN electronic:
978-1-62708-171-9
Publication date:
2013
Book Chapter

Renewable Energy Applications

By
Robert Vassen
Robert Vassen
Forschungszentrum Jülich Institute of Energy and Climate Research (IEK-1)
Search for other works by this author on:
Georg Mauer
Georg Mauer
Forschungszentrum Jülich Institute of Energy and Climate Research (IEK-1)
Search for other works by this author on:
Published:
2013
Page range:
318 - 321
Publication history
December 23, 2012

Abstract

The use of renewable energy has grown strongly in all end-use sectors such as power, heat, and transport. This article describes thermal spray applications that improve efficiency, lower maintenance costs, and prolong operational life in the renewable energy technologies, including wind power, hydro power, biomass and biofuels, solar energy, and fuel cells.

You do not currently have access to this content.
Don't already have an account? Register

Robert Vassen, Georg Mauer, 2013. "Renewable Energy Applications", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal