Thermal Spray Applications in the Paper Production Industry[1]

By
Mitchell R. Dorfman
Mitchell R. Dorfman
Revising author
Sulzer Metco (U.S.) Inc.
Search for other works by this author on:
Atin Sharma
Atin Sharma
Revising author
Sulzer Metco (U.S.) Inc.
Search for other works by this author on:
Published:
2013
Page range:
328 - 331
Publication history
March 25, 2013

Abstract

Thermal spray coatings, along with certain proprietary sealants, are widely used in the paper manufacturing industry for corrosion and wear resistance and to impart special surface characteristics. This article discusses the steps involved in the paper manufacturing process. Most modern papermaking machines are based on variations of the Fourdrinier machine. The article describes four operational sections of the machine: forming, press, drying, and calendar. It provides an overview of the machine components where thermal spray coatings are used, namely digesters, blow tanks, suction roll, center press rolls, yankee dryer rolls, calendar rolls, doctor/scalping blades, and cutting equipment.

You do not currently have access to this content.
Don't already have an account? Register

Mitchell R. Dorfman, Atin Sharma, 2013. "Thermal Spray Applications in the Paper Production Industry", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal