Skip to Main Content
ASM Handbook

Thermal Spray Technology

Edited by
Robert C. Tucker, Jr.
Robert C. Tucker, Jr.
The Tucker Group
Search for other works by this author on:
ASM International
Volume
5A
ISBN electronic:
978-1-62708-171-9
Publication date:
2013
Book Chapter

Thermal Spray Technology Growth in Gas Turbine Applications

By
Mitchell R. Dorfman
Mitchell R. Dorfman
Sulzer Metco (U.S.) Inc.
Search for other works by this author on:
D. Sporer
D. Sporer
Sulzer Metco (U.S.) Inc.
Search for other works by this author on:
P. Meyer
P. Meyer
Sulzer Metco (U.S.) Inc.
Search for other works by this author on:
Published:
2013
Page range:
280 - 286
Publication history
January 22, 2013

Abstract

This article provides an overview of key thermal spray coatings used in compressors, combustors, and turbine sections of a power-generation gas turbine. It describes the critical components, including combustors, transition ducts, inlet nozzle guide vanes, and first-stage rotating airfoils. Design requirements are reviewed and compared between aerospace and power generation coatings. Application process improvement areas are also discussed as a method of reducing component cost.

You do not currently have access to this content.
Don't already have an account? Register

Mitchell R. Dorfman, D. Sporer, P. Meyer, 2013. "Thermal Spray Technology Growth in Gas Turbine Applications", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal