Skip to Main Content
ASM Handbook

Thermal Spray Technology

Edited by
Robert C. Tucker, Jr.
Robert C. Tucker, Jr.
The Tucker Group
Search for other works by this author on:
ASM International
Volume
5A
ISBN electronic:
978-1-62708-171-9
Publication date:
2013
Book Chapter

Automotive Coatings and Applications

By
Noritaka Miyamoto
Noritaka Miyamoto
Toyota Motor Corporation
Search for other works by this author on:
Published:
2013
Page range:
298 - 305
Publication history
March 12, 2013

Abstract

This article describes the benefits that can be achieved by using thermal spray on particular engine parts of an automobile. These include improvement in fuel consumption, wear resistance and bonding, and reduction of oil consumption, exhaust heat loss, and cooling heat loss. Typical engine parts are cylinder blocks, cylinder bores, cast iron cylinder liners, piston rings, connecting rod bearings, turbochargers, engine valve lifters, exhaust system parts, and oxygen sensors. The article also describes the benefits of using thermal spray on transmission parts such as synchronizer rings and torque converters.

You do not currently have access to this content.
Don't already have an account? Register

Noritaka Miyamoto, 2013. "Automotive Coatings and Applications", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal