Coating Structures, Properties, and Materials

By
Daryl E. Crawmer
Daryl E. Crawmer
Thermal Spray Technologies Inc.
Search for other works by this author on:
Published:
2013
Page range:
60 - 64
Publication history
February 02, 2013

Abstract

This article provides information on thermal spray coating features, which combine to determine the properties of a coating. These include the lamellar or layered splat structure, entrapped unmelted or resolidified particles, pores, oxide inclusions, grains, phases, cracks, and bond interfaces. The article describes the sources of porosity and the factors that control the final coating porosity levels. The article also lists the materials most suitable for thermal spraying processes.

You do not currently have access to this content.
Don't already have an account? Register

Daryl E. Crawmer, 2013. "Coating Structures, Properties, and Materials", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal