Corrosion and Wear Control for Industrial Applications[1]

By
Mitchell R. Dorfman
Mitchell R. Dorfman
Revising author
Sulzer Metco (U.S.) Inc.
Search for other works by this author on:
Published:
2013
Page range:
257 - 261
Publication history
March 19, 2013

Abstract

This article focuses on noble and neutral coatings and the requirements necessary to achieve successful industrial applications. These include corrosion and wear control and repair applications in processing and chemical industries, and valve and downhole drilling applications in the petrochemical industry. The article also discusses substrate chemistry and preparation; coating selection process and microstructure; sealing by chemical, post-heat treatments, and laser processing; and thermal spray process alternatives.

You do not currently have access to this content.
Don't already have an account? Register

Mitchell R. Dorfman, 2013. "Corrosion and Wear Control for Industrial Applications", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal