Protective Overlays and Coatings Used in Oil Sands

By
Gary Fisher
Gary Fisher
Alberta Innovates—Technology Futures
Search for other works by this author on:
Tonya Wolfe
Tonya Wolfe
Alberta Innovates—Technology Futures
Search for other works by this author on:
Published:
2013
Page range:
312 - 317
Publication history
December 26, 2012

Abstract

This article focuses on coatings and overlays adopted for use as wear- and corrosion-resistant materials in oil sand processing. It describes the most common application processes for oil sand coatings and overlays, including welding, high-velocity oxyfuel thermal spray, laser cladding, and vacuum brazing. The article provides information on the selection of overlays and materials such as chromium-carbide-base overlays and tungsten carbide metal-matrix composites.

You do not currently have access to this content.
Don't already have an account? Register

Gary Fisher, Tonya Wolfe, 2013. "Protective Overlays and Coatings Used in Oil Sands", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal