Guidelines for the Use of Personal Protective Equipment in Thermal Spraying[1]

Published:
2013
Page range:
141 - 150
Publication history
March 14, 2013

Abstract

This article provides information on personal protective equipment (PPE), consistent with the Occupational Safety and Health Administration's Personal Protective Equipment Standard (29 CFR 1910.132-138). This standard is intended to protect individuals from the risk of injury by creating a barrier against workplace hazards. This article provides guidelines for establishing PPE programs with an overview of the responsibilities for employers, supervisors, and employees, assessing hazards associated with thermal spray operations, and training workers about PPE, as well as guidelines for selecting, using, and maintaining PPE. It presents an overview of eye, face, head, hand, foot, hearing, fall, and respiratory protection. Respiratory and hearing protection should be used in conjunction with industrial hygiene monitoring.

You do not currently have access to this content.
Don't already have an account? Register

2013. "Guidelines for the Use of Personal Protective Equipment in Thermal Spraying", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal