Skip to Main Content
ASM Handbook

Thermal Spray Technology

Edited by
Robert C. Tucker, Jr.
Robert C. Tucker, Jr.
The Tucker Group
Search for other works by this author on:
ASM International
Volume
5A
ISBN electronic:
978-1-62708-171-9
Publication date:
2013
Book Chapter

Additional Applications in Thermal Spray

By
Mitchell R. Dorfman
Mitchell R. Dorfman
Revising author
Sulzer Metco (U.S.) Inc.
Search for other works by this author on:
Published:
2013
Page range:
334 - 337
Publication history
March 19, 2013

Abstract

This article reviews the use of thermal spray polymer coatings as a replacement for paints. It discusses the applications of the thermal spray forming process. The article also provides information on the applications of thermal spray in metal processing, textile and plastics, and ceramic and glass manufacturing industries.

You do not currently have access to this content.
Don't already have an account? Register

Mitchell R. Dorfman, 2013. "Additional Applications in Thermal Spray", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal