Carbon Steels and Alloy Steels Used in Warm and Hot Working

By
Chester J. Van Tyne
Chester J. Van Tyne
Colorado School of Mines
Search for other works by this author on:
Kester D. Clarke
Kester D. Clarke
Los Alamos National Laboratory
Search for other works by this author on:
Published:
2014
Page range:
302 - 305
Publication history
May 27, 2014

Abstract

This article focuses on the specific features of carbon steels and alloy steels that are pertinent to heating by induction for warm and hot working processes. It provides a detailed account of the effects of various microstructures on austenitization kinetics for AISI 1045 steels. The article explains the factors to be considered for induction heating of various steel alloys. It describes the temperature and compositional issues that should be considered in the forging of steels that are induction heated.

You do not currently have access to this content.
Don't already have an account? Register

Chester J. Van Tyne, Kester D. Clarke, 2014. "Carbon Steels and Alloy Steels Used in Warm and Hot Working", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal