Skip to Main Content
ASM Handbook

Induction Heating and Heat Treatment

Edited by
Valery Rudnev
Valery Rudnev
Inductoheat Inc.
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4C
ISBN electronic:
978-1-62708-167-2
Publication date:
2014
Book Chapter

Metallurgy of Induction Melting Processes for Iron and Non-Iron Materials

By
Erwin Dötsch
Erwin Dötsch
ABP Induction Systems
Search for other works by this author on:
Published:
2014
Page range:
474 - 490
Publication history
May 27, 2014

Abstract

Interplays of metallurgical factors, such as dissolved oxygen, carbon, and silicon content, that control the molten metal from melting to pouring, have a decisive influence on the quality of the castings. This article focuses on the magnesium treatment and desulfurization carried out during inoculation and nucleation of molten cast iron, assisting in the formation of cast iron. The different types of cast irons are gray cast iron, nodular cast iron, compacted graphite iron, malleable cast iron, and alloyed cast iron. The article provides an overview of the melt treatment processes carried out in cast steel, wrought and cast aluminum, and copper materials.

You do not currently have access to this content.
Don't already have an account? Register

Erwin Dötsch, 2014. "Metallurgy of Induction Melting Processes for Iron and Non-Iron Materials", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal