Skip to Main Content
ASM Handbook

Induction Heating and Heat Treatment

Edited by
Valery Rudnev
Valery Rudnev
Inductoheat Inc.
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4C
ISBN electronic:
978-1-62708-167-2
Publication date:
2014
Book Chapter

Controlled Atmosphere Chambers

By
Scott Larrabee
Scott Larrabee
Radyne Corporation
Search for other works by this author on:
Published:
2014
Page range:
691 - 700
Publication history
May 27, 2014

Abstract

Controlled atmosphere chambers are used to control the surface chemistry of the metals that are being processed. This article focuses on the various types of controlled atmospheres used in induction heat treating and brazing, namely, inert gas atmospheres based on argon and helium; prepared and commercial nitrogen-base atmospheres; and brazing atmospheres. It provides detailed information on two types of controlled atmosphere chambers: atmosphere and vacuum. The article also describes the selection factors, advantages, and disadvantages of these chambers.

You do not currently have access to this content.
Don't already have an account? Register

Scott Larrabee, 2014. "Controlled Atmosphere Chambers", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal