Components, Design, and Operation of Vacuum Induction Crucible Furnaces

By
Egbert Baake
Egbert Baake
Leibniz University of Hannover
Search for other works by this author on:
Published:
2014
Page range:
462 - 466
Publication history
May 27, 2014

Abstract

This article discusses the principle, coil design, types and operation of a vacuum induction furnace. It describes the operation parameters that should be considered during the functioning of the induction furnace.

You do not currently have access to this content.
Don't already have an account? Register

Egbert Baake, 2014. "Components, Design, and Operation of Vacuum Induction Crucible Furnaces", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal