Skip to Main Content
ASM Handbook

Induction Heating and Heat Treatment

Edited by
Valery Rudnev
Valery Rudnev
Inductoheat Inc.
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4C
ISBN electronic:
978-1-62708-167-2
Publication date:
2014
Book Chapter

Temperature Requirements for Heating Titanium, Aluminum, Magnesium, and Copper Alloys

By
Alexey Sverdlin
Alexey Sverdlin
Bradley University
Search for other works by this author on:
Published:
2014
Page range:
313 - 329
Publication history
May 27, 2014

Abstract

This article focuses on the temperature requirements of typical nonferrous metals and their alloys of commercial importance. These include aluminum, copper, magnesium, and titanium. The article describes the thermoelectricity, photoelectricity, and capacity of aluminum alloys. In addition, it provides information on the electrical properties of copper and its alloys. The article also lists typical physical and mechanical properties of aluminum alloys at ambient temperature.

You do not currently have access to this content.
Don't already have an account? Register

Alexey Sverdlin, 2014. "Temperature Requirements for Heating Titanium, Aluminum, Magnesium, and Copper Alloys", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal