Book Chapter

Metallurgy of Induction Hardening of Steel

By
David K. Matlock
David K. Matlock
Colorado School of Mines
Search for other works by this author on:
Published:
2014
Page range:
45 - 57
Publication history
May 27, 2014

Abstract

This article focuses on induction hardening process for heat treating operations specifically designed to result in proper microstructure/property combinations in either localized or in the final parts. It briefly reviews the heat treating basics for conventional heat treating operations of steels with iron-carbon phase and transformation diagrams. The article provides a summary of the important temperatures, definitions, and microstructural constituents associated with heat-treated steels. Basic transformation characteristics of heat-treated steels are reviewed. The article also discusses the various aspects of steel heat treatment by induction processing, and concludes with a description of steel alloys for induction processing.

You do not currently have access to this content.
Don't already have an account? Register

David K. Matlock, 2014. "Metallurgy of Induction Hardening of Steel", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten