Skip to Main Content
ASM Handbook

Induction Heating and Heat Treatment

Edited by
Valery Rudnev
Valery Rudnev
Inductoheat Inc.
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4C
ISBN electronic:
978-1-62708-167-2
Publication date:
2014
Book Chapter

Temperature Requirements for Heating Super Alloys and Stainless Steels

By
David U. Furrer
David U. Furrer
Pratt & Whitney
Search for other works by this author on:
Published:
2014
Page range:
306 - 312
Publication history
May 27, 2014

Abstract

This article discusses special considerations relative to induction heating of stainless steels and nickel-base superalloys. It focuses on the various industrial and high-temperature applications of induction heating to stainless steel and superalloy components, namely, primary melting processes, preheating for primary and secondary forming processes, heat treatments, brazing, and thermal processing for fusion welds. The article also provides information on computational modeling of induction heating processes for super alloys and stainless steels.

You do not currently have access to this content.
Don't already have an account? Register

David U. Furrer, 2014. "Temperature Requirements for Heating Super Alloys and Stainless Steels", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal