Skip to Main Content
ASM Handbook

Induction Heating and Heat Treatment

Edited by
Valery Rudnev
Valery Rudnev
Inductoheat Inc.
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4C
ISBN electronic:
978-1-62708-167-2
Publication date:
2014
Book Chapter

Vertical Scanners, Horizontal Scanners, and Tooth by Tooth Scanners

By
Ronald R. Akers
Ronald R. Akers
Ajax Tocco Magnethermic
Search for other works by this author on:
Published:
2014
Page range:
683 - 690
Publication history
May 27, 2014

Abstract

Scanners are the most versatile and flexible of the equipment available to the heat treating industry for induction hardening. This article provides a general overview of scanners, and describes various critical factors, including scan speeds, rotational speeds, and center total indicator runout of vertical scanners. It presents information on the frequency selection parameters for scanning applications. The article also discusses the critical parameters and production rates in specifying and developing a tooth-by-tooth hardening process.

You do not currently have access to this content.
Don't already have an account? Register

Ronald R. Akers, 2014. "Vertical Scanners, Horizontal Scanners, and Tooth by Tooth Scanners", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal