Skip to Main Content
ASM Handbook

Heat Treating of Nonferrous Alloys

Edited by
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4E
ISBN electronic:
978-1-62708-169-6
Publication date:
2016
Book Chapter

Effect of Heat Treatment on Mechanical Properties of Titanium Alloys[1]

By
Rodney R. Boyer
Rodney R. Boyer
Revising author
RBTi Consulting
Search for other works by this author on:
John Foltz
John Foltz
Revising author
ATI
Search for other works by this author on:
Published:
2016
Page range:
555 - 572
Publication history
November 11, 2016

Abstract

The response of titanium and titanium alloys to heat treatment depends on the composition of the metal, the effects of the alloying elements on the alpha-beta crystal transformation, and the thermomechanical processing utilized during processing of the alloy. This article provides a detailed discussion on the effects of heat treatment on the mechanical properties for three general classes of titanium alloys, namely, alpha and near-alpha titanium alloys, alpha-beta alloys, and beta alloys.

You do not currently have access to this content.
Don't already have an account? Register

Rodney R. Boyer, John Foltz, 2016. "Effect of Heat Treatment on Mechanical Properties of Titanium Alloys", Heat Treating of Nonferrous Alloys, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal