Skip to Main Content
ASM Handbook

Heat Treating of Nonferrous Alloys

Edited by
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4E
ISBN electronic:
978-1-62708-169-6
Publication date:
2016
Book Chapter

Heat Treating of Bronzes

By
Sabit Ali
Sabit Ali
NBM Metals, Inc.
Search for other works by this author on:
Published:
2016
Page range:
355 - 396
Publication history
November 11, 2016

Abstract

Bronzes generally are used to describe many different copper-base alloys in which the major alloying addition is neither zinc nor nickel. They are generally classified by their major alloying elements, for example, tin bronzes with phosphorus used as a deoxidizer, aluminum bronzes, nickel-aluminum bronzes, silicon bronzes, and beryllium bronzes. This article briefly discusses the types, hardening mechanisms, heat treatment processes, applications, and mechanical properties of these bronzes and high-copper alloys.

You do not currently have access to this content.
Don't already have an account? Register

Sabit Ali, 2016. "Heat Treating of Bronzes", Heat Treating of Nonferrous Alloys, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal