Skip to Main Content
ASM Handbook

Heat Treating of Nonferrous Alloys

Edited by
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4E
ISBN electronic:
978-1-62708-169-6
Publication date:
2016
Book Chapter

Heat Treatment of Cast Nickel-Base Alloys

By
John Marcin
John Marcin
Rensselaer at Hartford
Search for other works by this author on:
Matthew Donachie
Matthew Donachie
Rensselaer at Hartford
Search for other works by this author on:
Published:
2016
Page range:
459 - 478
Publication history
November 11, 2016

Abstract

Cast nickel-base alloys are used extensively in corrosive-media and high-temperature applications. This article briefly reviews the common types of heat treatments of nickel alloy castings: homogenization, stress relieving, in-process annealing, full annealing, solution annealing, quenching, coating diffusion, and precipitation. It describes the three general strengthening mechanisms, namely, solid-solution hardening, age hardening, and carbide precipitation. The article summarizes the typical heat treatment of the general families of nickel-base castings used in industrial applications. It focuses on the solution treatment and age hardening of cast nickel-base superalloys and the heat treatment of cast solid-solution alloys for corrosion-resisting applications. The article also discusses the typical types of atmospheres used in annealing or solution treating: exothermic, endothermic, dry hydrogen, dry argon, and vacuum.

You do not currently have access to this content.
Don't already have an account? Register

John Marcin, Matthew Donachie, 2016. "Heat Treatment of Cast Nickel-Base Alloys", Heat Treating of Nonferrous Alloys, George E. Totten