Heat Treatable Nonferrous Alloys

By
Alexey Sverdlin
Alexey Sverdlin
Milwaukee School of Engineering
Search for other works by this author on:
Steven Lampman
Steven Lampman
ASM International
Search for other works by this author on:
Published:
2016
Page range:
44 - 62
Publication history
November 11, 2016

Abstract

This article describes the different types of precipitation and transformation processes and their effects that can occur during heat treatment of various nonferrous alloys. The nonferrous alloys are aluminum alloys, copper alloys, magnesium alloys, nickel alloys, titanium alloys, cobalt alloys, zinc alloys, and heat treatable silver alloys, gold alloys, lead alloys, and tin alloys. It also provides a detailed discussion on the effects due to precipitation and transformation processes in these non-ferrous alloys.

You do not currently have access to this content.
Don't already have an account? Register

Alexey Sverdlin, Steven Lampman, 2016. "Heat Treatable Nonferrous Alloys", Heat Treating of Nonferrous Alloys, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal