Heat Treatment of Aluminum Alloy Castings

By
Geoffrey K. Sigworth
Geoffrey K. Sigworth
Consultant
Search for other works by this author on:
Published:
2016
Page range:
274 - 288
Publication history
November 11, 2016

Abstract

This article presents a detailed discussion on typical thermal treatment practices for hardening of various aluminum casting alloys. These practices are solution treatment, quenching or cooling, preaging, and artificial aging at an elevated temperature. The aluminum casting alloys considered here are: Al-Cu and Al-Cu-Mg (2xx) alloys, Al-Zn-Mg (7xx) alloys, Al-Si-Mg alloys, Al-Si-Cu, and Al-Si-Cu-Mg alloys.

You do not currently have access to this content.
Don't already have an account? Register

Geoffrey K. Sigworth, 2016. "Heat Treatment of Aluminum Alloy Castings", Heat Treating of Nonferrous Alloys, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal