Book Chapter

Heat Treating of Titanium and Its Alloys

Published:
2016

Abstract

This article introduces the different types, distinctions, and grades of commercially pure titanium and titanium alloys. It describes three types of alloying elements: alpha stabilizers, beta stabilizers, and neutral additions. The article discusses the basic categories of titanium alloys, namely, alpha and near-alpha titanium alloys, beta and near-beta titanium alloys, and alpha-beta titanium alloys. It also describes the general microstructural features of titanium alloys.

Abstract

This article provides a detailed discussion on the heat treatment processes for titanium and titanium alloys. These processes are age hardening, solution treatment, aging, and annealing. The article illustrates the characteristics of equilibrium phase diagrams that are important for understanding the heat treatment of titanium alloys. It explains the types of metastable phases encountered in titanium alloys. The article also provides information on the equilibrium phase relationships and properties of titanium alloys.

You do not currently have access to this content.
Don't already have an account? Register

2016. "Heat Treating of Titanium and Its Alloys", Heat Treating of Nonferrous Alloys, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal