Journal Articles
AM&P Technical Articles (2018) 176 (7): 16–20.
Published: 01 October 2018
...Francis H. (Sam) Froes New methods for processing titanium alloys offer the potential to enhance mechanical properties while reducing component cost. This article discusses innovative and potentially lower cost fabrication processes including additive manufacturing (AM), superplastic forming...
Journal Articles
AM&P Technical Articles (2014) 172 (2): 18–23.
Published: 01 February 2014
...B. Dutta; F.H. (Sam) Froes Although the widespread use of titanium alloys is constrained by high costs, powder metallurgy techniques such as additive manufacturing (AM) represent an economical approach to fabricating titanium components. Various approaches to AM, along with examples of components...
Journal Articles
AM&P Technical Articles (2018) 176 (3): 18–24.
Published: 01 April 2018
...Francis H. (Sam) Froes; Ashraf Imam Among the structural materials developed in the 20th century, titanium and its alloys have played a leading role in improving component performance. This article discusses development of new production techniques, specifications, economic aspects...
Journal Articles
AM&P Technical Articles (2015) 173 (8): 46–47.
Published: 01 September 2015
...Stanley Abkowitz This communication is a response to the April 2015 Metallurgy Lane article, Titanium, Part II, by Charles Simcoe. This present piece offers differing historical evidence about the development and commercialization of titanium alloys, including discussion of the patent office...
Journal Articles
AM&P Technical Articles (2015) 173 (9): 48.
Published: 01 October 2015
... professor of mechanical engineering and technical director of CHTE. Titanium and titanium alloys, cobalt alloys, and stainless steels are the four main types of metallic biomaterials. Titanium alloys are preferred in dental and orthopedic implants due to their good mechanical properties, biocompatibility...
Journal Articles
AM&P Technical Articles (2016) 174 (4): 21–24.
Published: 01 April 2016
...John Foltz; Rick Hugo High-speed, high-fidelity techniques used to analyze texture and dislocation content enable greater understanding of the influence of texture on deformation of titanium alloys than previously possible. This article describes a study in which specimens were examined using...
Journal Articles
AM&P Technical Articles (2024) 182 (2): 20–23.
Published: 01 March 2024
...Vasisht Venkatesh; Adam Pilchak The 15th World Conference on Titanium included papers on titanium alloy development, efforts to reduce Ti powder costs, additive manufacturing, and computational materials modeling tools. This article reviews some of the key advances reported at the conference...
Journal Articles
AM&P Technical Articles (2023) 181 (1): 12–20.
Published: 01 January 2023
... components to make in-field repairs at the point of need. The focus of the initial research was aluminum alloys. Preliminary studies show significant promise for the adaptation of these techniques to hard alloys including steel castings, wrought high strength steels, and titanium alloys. This article...
Journal Articles
AM&P Technical Articles (2020) 178 (3): 22–25.
Published: 01 April 2020
...Gregory Vartanov High-strength, corrosion-resistant steel is proposed as a cost-effective alternative to titanium alloys due to its high specific strength, high fatigue strength, good toughness, and corrosion resistance. High-strength, corrosion-resistant steel is proposed as a cost-effective...
Journal Articles
AM&P Technical Articles (2021) 179 (3): 14–18.
Published: 01 April 2021
...Michelle Harr; Adam Pilchak; Lee Semiatin Despite decades of research, fundamental questions still exist regarding the role of microtexture on the deformation, fatigue, and fracture behavior of titanium alloys. This article describes the microstructural evolution processes that result...
Journal Articles
AM&P Technical Articles (2021) 179 (6): 13–18.
Published: 01 September 2021
...Michelle Harr; Adam Pilchak; Lee Semiatin This article, the second in a two-part series on titanium alloys, examines the effects of microtexture on deformation behavior, slip dislocations, and fatigue properties. Part I, which appeared in the April 2021 issue, described microstructural evolution...
Journal Articles
AM&P Technical Articles (2016) 174 (5): 37–39.
Published: 01 May 2016
...Vasisht Venkatesh; Rodney Boyer Developments in titanium technology and opportunities for increased use in several markets were highlighted at the 13th World Conference on Titanium. This article reviews some of the key technical topics covered at the conference, including new alloy development...
Journal Articles
AM&P Technical Articles (2018) 176 (2): 19–25.
Published: 01 February 2018
...Francis H. (Sam) Froes; Ashraf Imam Among the structural materials developed in the 20th century, titanium and its alloys have played a leading role in improving component performance. This article provides background on the extraction and primary processing of titanium. Among the structural...
Journal Articles
AM&P Technical Articles (2015) 173 (5): 28–29.
Published: 01 May 2015
... by government and industry, titanium fulfilled its promise as a new metal for jet engine and airframe applications. Copyright © ASM International® 2015 2015 ASM International aerospace materials titanium alloys ADVANCED MATERIALS & PROCESSES | MAY 2015 httpsdoi.org/10.31399/asm.amp.2015-05...
Journal Articles
AM&P Technical Articles (2017) 175 (5): 36–40.
Published: 01 July 2017
... discusses the basics of AM, part design considerations, CAD models, and build and powder removal considerations. Copyright © ASM International® 2017 2017 ASM International additive manufacturing aerospace components titanium alloy parts httpsdoi.org/10.31399/asm.amp.2017-05.p036 36...
Journal Articles
AM&P Technical Articles (2012) 170 (9): 16–22.
Published: 01 September 2012
... atomized powders powder metallurgy sponge fines titanium powder titanium alloys httpsdoi.org/10.31399/asm.amp.2012-09.p016 Titanium Powder Metallurgy: A Review Part 1 F.H. (Sam) Froes, FASM* Tacoma, Wash. Titanium and its alloys are the materials of choice for many applications, but high cost...
Journal Articles
AM&P Technical Articles (2012) 170 (10): 26–29.
Published: 01 October 2012
... powder-injection molding prealloyed titanium powder spray forming tensile properties titanium alloys httpsdoi.org/10.31399/asm.amp.2012-10.p026 Titanium Powder Metallurgy: A Review Part 2 F.H. (Sam) Froes, FASM* Tacoma, Wash. Titanium and its alloys are the materials of choice for many...
Journal Articles
AM&P Technical Articles (2021) 179 (3): 19–22.
Published: 01 April 2021
... titanium extrusions for applications beyond the long structural components of an aircraft. Copyright © ASM International® 2021 2021 ASM International aircraft components near net shape extrusion titanium alloys httpsdoi.org/10.31399/asm.amp.2021-03.p019 19 ADVANCED MATERIALS & PROCESSES...
Journal Articles
AM&P Technical Articles (2015) 173 (3): 28–29.
Published: 01 March 2015
... titanium alloys httpsdoi.org/10.31399/asm.amp.2015-03.p028 28 TECHNICAL SPOTLIGHT ADVANCED MATERIALS & PROCESSES | MARCH 2015 ADDITIVE MANUFACTURING MAKES TITANIUM USE MORE FEASIBLEitanium, the ninth most abundant element in the earth s crust, holds Tthe highest strength-to-weight levels, powder cost...
Journal Articles
AM&P Technical Articles (2013) 171 (10): 15–17.
Published: 01 October 2013
... impact performance. Titanium alloys are widely used in aerospace applications due to their excellent specific strength and fatigue properties[1-3]. Among these materials, Ti-6Al-4V (Ti64) is the most widely used alloy and consists of a beta phase rich in vanadium with a crystallographic bcc structure...