AM&P Technical Articles (2013) 171 (7): 22–26.
Published: 01 July 2013
...S. Yadavali; R. Kalyanaraman This article provides an overview of pulsed laser dewetting self-assembly (PLDSA) and its use in the production of silver and cobalt films with desired nanostructure. This article provides an overview of pulsed laser dewetting self-assembly (PLDSA) and its use...