Journal Articles
AM&P Technical Articles (2021) 179 (3): 14–18.
Published: 01 April 2021
...Michelle Harr; Adam Pilchak; Lee Semiatin Despite decades of research, fundamental questions still exist regarding the role of microtexture on the deformation, fatigue, and fracture behavior of titanium alloys. This article describes the microstructural evolution processes that result...
Journal Articles
AM&P Technical Articles (2021) 179 (6): 13–18.
Published: 01 September 2021
...Michelle Harr; Adam Pilchak; Lee Semiatin This article, the second in a two-part series on titanium alloys, examines the effects of microtexture on deformation behavior, slip dislocations, and fatigue properties. Part I, which appeared in the April 2021 issue, described microstructural evolution...
Journal Articles
AM&P Technical Articles (2016) 174 (5): 37–39.
Published: 01 May 2016
..., are combining electron backscatter diffraction (EBSD) orientation maps and high resolution DIC to observe nanoscale strain behavior in Ti-6Al-4V with varying degrees of microtexture. Two extreme microstructures show noticeable differences in strain heterogeneity, with the strong microtexture sample exhibiting...
Journal Articles
AM&P Technical Articles (2024) 182 (2): 20–23.
Published: 01 March 2024
... reported at the conference. additive manufacturing computational materials modeling tools microtexture titanium titanium alloys titanium powder 2 0 httpsdoi.org/10.31399/asm.amp.2024-02.p020 ADVANCED MATERIALS & PROCESSES | MARCH 2024 A SUMMARY OF Ti-2023: THE WORLD CONFERENCE ON TITANIUM...
Journal Articles
AM&P Technical Articles (2019) 177 (2): 38–41.
Published: 01 February 2019
... International® 2019 2019 ASM International corrosion protection microtexturing thermal spray coating wear protection httpsdoi.org/10.31399/asm.amp.2019-02.p038 38 iTSSe TSS FEATURE ADVANCED MATERIALS & PROCESSES | FEBRUARY/MARCH 2019 THERMAL SPRAY IMPACTS MULTIPLE INDUSTRIES The use of coatings...
Journal Articles
AM&P Technical Articles (2013) 171 (3): 32–34.
Published: 01 March 2013
...., Combined micro and macro additive manufacturing of a swirling flow coaxial phacoemulsifier sleeve with internal micro-vanes, Biomedical Microdevices, 12, p 875-886, 2010. 18. A. Schneider, et al., Biomimetic microtexturing for neurosurgical probe surfaces to influence tribological characteristics during...
Journal Articles
AM&P Technical Articles (2017) 175 (6): 18–22.
Published: 01 September 2017
... if the shortfall will affect the part s function. These analyses can be time consuming and expensive, and they limit the number of parts that can be Fig. 2 Schematic of direct energy deposition (DED) process. manufactured via AM. This epitaxial growth can result in a microtexture, which could Fig. 3 Schematic...
Journal Articles
AM&P Technical Articles (2019) 177 (1): 16–21.
Published: 01 January 2019
.... References 1. M.N. Alam and M. Blackman, HighAngle Kikuchi Patterns, Proc. Royal Soc. of London A: Mathematical, Physical and Engineering Sciences, 221(1145), p 224-242, 1954. 2. D.J. Dingley and V. Randle, Microtexture Determination by Electron Backscatter Diffraction, J. Matls. Sci., 27(17), p 4545-4566...