1-9 of 9 Search Results for

composite coil springs

Sort by
Journal Articles
AM&P Technical Articles (2013) 171 (6): 15–17.
Published: 01 June 2013
...Aleksander Koprivc This article discusses the capabilities of a compression test system developed to evaluate composite coil springs for automotive suspension systems. This article discusses the capabilities of a compression test system developed to evaluate composite coil springs...
Journal Articles
AM&P Technical Articles (2016) 174 (3): 30–31.
Published: 01 March 2016
... technology. The first breakthrough came when a member of the team, Steven Copley, was making a coiled spring to study the properties of DS crystals. He used a mold in the shape of a coiled spring suspended in liquid metal with DS crystals growing from the bottom of the regular water-cooled plate...
Journal Articles
AM&P Technical Articles (2015) 173 (3): 18–23.
Published: 01 March 2015
... springs. Glass fiber-epoxy composite springs are used in the front while hollow steel springs are used in the rear. The composite front spring weighs 1.2 kg vs 2.8 kg a 57% savings. The hollow steel rear spring reduces the weight by 1.6 kg and results in a 37% savings (from 2.7 kg vs 4.3 kg). An 11 kg...
Journal Articles
AM&P Technical Articles (2016) 174 (1): 30–33.
Published: 01 January 2016
..., Minn. A guidewireisamedicaldeviceused in various minimally invasive vascular applications. Its foundation is a metal core wire, typically constructed of stainless steel or Nitinol. A metal coil, polymer jacket, or combination of the two covers the core wire on the distal end in order to make the tip...
Journal Articles
AM&P Technical Articles (2013) 171 (9): 26–30.
Published: 01 September 2013
... 4098 gas turbine engine. Fig. 2 Grain boundary failure. Under jet engine operating conditions, failure occurs at crystal boundaries. 26 ADVANCED MATERIALS & PROCESSES SEPTEMBER 2013 TABLE I NICKEL BASE SUPERALLOY COMPOSITIONS [wt%] Alloy Cr Co W Ti Al C B Zr Udimet-700 15.0 15.3 3.4 4.30 0.070...
Journal Articles
AM&P Technical Articles (2018) 176 (5): 18–24.
Published: 01 July 2018
... outer panel weight. Alloy X5020 (2.8%Mg-1.6%Cu-0.3%Mn) was a truly unique, heat treatable composition offering a better combination of after-bake strength and formability compared to 2036. This alloy was apparently aimed at an improved recycling compatibility with 2036 outers. Alloy X5085 (6.2%Mg-0.2%Mn...
Journal Articles
AM&P Technical Articles (2022) 180 (4): 49–62.
Published: 01 May 2022
... Commendation Award, VT Outstanding Student Award, NITW Sri Kabadi Subalu Medal, and the NITW Alumni Association Gold Medal. Mr. John C. Kuli, Jr. Nominee for Treasurer John C. Kuli, Jr., is technology and innovation lead for operations within the Performance Alloys & Composites Division of Materion. His...
Journal Articles
AM&P Technical Articles (2020) 178 (4): 67–78.
Published: 01 May 2020
... for new materials and processes in rer, FASM, and trustees Prem K. Aurora and Dr. Thomas M. the jet engine industry. Her research at TRW was in a wide Moore, FASM. Dr. Judith Todd, FASM, has completed her range of composites systems including design, manufac- term as trustee and is now vice president...
Journal Articles
AM&P Technical Articles (2021) 179 (4): 66–77.
Published: 01 May 2021
... societies in materials, microscopy, and aerospace. Mr. John C. Kuli, Jr. Nominee for Treasurer John C. Kuli, Jr., is technology and innovation lead for operations within the Performance Alloys & Composites Division of Materion. His present role is focused on upgrading existing equipment and purchasing new...