AM&P Technical Articles (2012) 170 (3): 28–30.
Published: 01 March 2012
...D. Anantha Padmanaban; Gulshan Kurien Aluminum-silicon (Al-Si) alloys have good castability in combination with high corrosion resistance, thermal conductivity, and specific strength, making them a strong candidate for many automotive applications. This article describes the processes used...
Journal Articles
AM&P Technical Articles (2013) 171 (9): 17–19.
Published: 01 September 2013
... of advanced alloys with improved performance, at a significantly lower cost than historical methods. Examples of ICME-designed alloys include: Castable titanium with properties that exceed those of wrought Ti-6-4 (produced using 75% Ti-6-4 scrap stream) Greater ductility, higher DBTT, and thermally-stable...
Journal Articles
AM&P Technical Articles (2015) 173 (1): 26–30.
Published: 01 January 2015
... is the most widely used alloying addition in magnesium for strengthening and castability. Figure 1(a) shows the calculated Mg-Al phase diagram. Two eutectic reactions are important to the phase constitution of Mg-Al binary alloys: *Member of ASM International engineering (ICME) tools used in the development...
Journal Articles
AM&P Technical Articles (2013) 171 (9): 26–30.
Published: 01 September 2013
... great castability. Ta was a great element all around, as it provided good strengthening, castability, and oxidation resistance. The alloy developed to fit the bill was PWA1480. Fortunately, improved coating chemistries and processes were developed as well. The Air Force Office of Scientific Research...
Journal Articles
AM&P Technical Articles (2018) 176 (6): 46–49.
Published: 01 September 2018
.... An encased coil using a castable refractory noise does not reach an appreciable level. Therefore, there is (for example, special grades of cement) offers durabili- no reason to be concerned about excessive noise, although ty and longer life, eliminating or dramatically reducing there are a few exceptions...
Journal Articles
AM&P Technical Articles (2024) 182 (4): 29–32.
Published: 01 May 2024
... is an alloy notoriously difficult to forge, system (e.g., tilt-furnace) for pouring molten metal, the timing and weights are meticulously con- trolled; consistency and effi- ciencies are improved[8]. Tin bronze is a castable alloy which has a wide solidification tem- perature range (150° 300°F)[9...
Journal Articles
AM&P Technical Articles (2018) 176 (4): 16–21.
Published: 01 May 2018
... structural applications for magnesium[1]. This is due to the excellent castability of magnesium alloys, which exceeds other metals such as aluminum and copper. Magnesium s unique solidification features, including high fluidity and low susceptibility to hydrogen porosity, make it a good candidate...
Journal Articles
AM&P Technical Articles (2014) 172 (3): 15–19.
Published: 01 March 2014
... than aluminum), Mg alloys are attractive to both the aerospace and automotive industries due to their high strength-to-weight ratio, good castability, high impact resistance, and high recyclability. However, its high oxidation potential usually results in inclusion contents much greater than that found...
Journal Articles
AM&P Technical Articles (2019) 177 (4): 14–19.
Published: 01 May 2019
.... A recent trial included new high entropy alloys[7]. The major portion of today s alloys used for the thermomechanical route of billet preparation are casting grades. The most common ones are aluminum casting alloys A356 and A357, both having good fluidity and castability due to their high content of Al-Si...
Journal Articles
AM&P Technical Articles (2021) 179 (4): 15–21.
Published: 01 May 2021
... Environmental Design of Cost-Effective, HighTemperature, Sensible Thermal Energy Storage Using Industrial Byproducts Massachusetts Institute of Technology Powdermet Ceramic Castable Cement Tanks and Piping for Molten Salt High-Toughness Cermets for Molten Salt Pumps URL link httpswww.energy.gov/eere/solar/seto...
Journal Articles
AM&P Technical Articles (2018) 176 (4): 47–56.
Published: 01 May 2018
... of high strength steels for structural and power transmission applications; precipitation strengthened cobalt-base alloys; alloys for additive manufacturing; nontoxic, high strength/low friction copper-base alloys to replace lead-containing bronzes; a low cost, castable titanium alloy; a highly...