AM&P Technical Articles (2012) 170 (8): 25–27.
Published: 01 August 2012
...Keith Ferguson Active metal brazing played a key role in the development and fabrication of a modified beam target for particle-physics experiments conducted by Fermilab. The new target consists of a titanium tube filled with stacked graphite fins that were bonded in place by means of active metal...
Journal Articles
AM&P Technical Articles (2014) 172 (7): 15–19.
Published: 01 July 2014
...Craig Moller; Jim Grann Successful part brazing relies on proper joint design, part cleanliness, and correct fixturing of part assemblies. Routine furnace maintenance allows repeatable, quality brazing results over time. This article describes aluminum brazing processes and process control...
Journal Articles
AM&P Technical Articles (2017) 175 (7): 25–29.
Published: 01 October 2017
...Anming Hu; Denzel Bridges; Suhong Zhang; Zhili Feng Nanobrazing is an innovative brazing technique that uses nanomaterials as the filler materials. Incorporating nanobrazing into conventional technologies such as vacuum and laser brazing creates a new frontier for repairing turbine blades and vanes...
Journal Articles
AM&P Technical Articles (2012) 170 (1): 24–27.
Published: 01 January 2012
...Edward D. Herderick; Kirk Cooper; Nate Ames A novel brazing approach for joining SiC-based fuel cladding is a promising technology for enhanced accident-tolerant nuclear fuels. A novel brazing approach for joining SiC-based fuel cladding is a promising technology for enhanced accident-tolerant...
Journal Articles
AM&P Technical Articles (2012) 170 (8): 22–24.
Published: 01 August 2012
... tank and presents examples in which it was used to detect delaminations in solar panels and clogs in brazed aluminum-copper cooling-ring assemblies. It also explains how to deal with issues that arise when scanning large-area parts. Acoustic micro imaging is widely used for inspecting IC packages...
Journal Articles
AM&P Technical Articles (2015) 173 (9): 56–60.
Published: 01 October 2015
... such as workpiece geometry, temperature uniformity and required heat pattern, and production rate, among others. Alternating current flowing in the inductor generates a time-varying magnetic field that FABRICATION TECHNIQUES Two traditional techniques used to fabricate hardening inductors are banding and brazing...
Journal Articles
AM&P Technical Articles (2012) 170 (2): 18–19.
Published: 01 February 2012
... tube energy dispersive X-ray spectroscopy joint fabrication microstructural analysis silver brazing silver plating httpsdoi.org/10.31399/asm.amp.2012-02.p018 JACQUET-LUCAS AWARD Microstructural Analysis of a Silver Plated-Brass Trombone Christopher Marvel* Will Lenthe John Logan Lehigh...
Journal Articles
AM&P Technical Articles (2021) 179 (3): 37–38.
Published: 01 April 2021
... heat sinks. In such a concept, the portion of the heat sink that comes in contact with the electronic device is made of copper, while the other portion is made of cheaper and lighter aluminum. However, joining aluminum and copper is a difficult challenge. Soldering and brazing is commonly used to join...
Journal Articles
AM&P Technical Articles (2020) 178 (4): 27–30.
Published: 01 May 2020
... alloy to form a near net shape bit body[4]. The infiltrated matrix body is then broken out from the graphite preform, cleaned, and attached to API threading. PDC cutters are brazed into their respective pockets and the bit is sent for final inspection and painting. A bit body with PDC cutters is shown...
Journal Articles
AM&P Technical Articles (2013) 171 (9): 59–61.
Published: 01 September 2013
... shape distortion and causing nonuniform hardness profiles around the perimeter. In addition, Ushaped inductors are fabricated either by banding or brazing copper in the shape of a figure eight containing multiple bands/joints (Fig. 2, top). Both coil fabrication methods raise concerns about the *Member...
Journal Articles
AM&P Technical Articles (2024) 182 (3): 33–36.
Published: 01 April 2024
... clad structure Ceramic-metal bonding GTV K2 HVOF JOINING TECHNOLOGIES HVOF coatings can support joining processes like brazing, soldering, and welding in several ways as summarized in Table 3[3]. Coatings produced by the liquid fuel HVOF GTV K2 torch are typically formed by spraying particles...
Journal Articles
AM&P Technical Articles (2016) 174 (1): 22–25.
Published: 01 January 2016
... added molten metal at increased temperatures, generally much higher than room temperature[1]. Similarly, welding and brazing also involve high-temperature melting, where brazing refers to joining through added molten metal at even higher temperatures than soldering, and welding involves melting...
Journal Articles
AM&P Technical Articles (2018) 176 (2): 58–61.
Published: 01 February 2018
..., end heating, brazing, and selective 8 hardening. More energy e icient and environmentally friendly than other heating methods including gas-fired furnaces, salt and lead baths, and carburizing and nitriding systems. Advantages in safety (no combustion or environmental contaminants), reduced labor...
Journal Articles
AM&P Technical Articles (2023) 181 (3): 20–22.
Published: 01 April 2023
... components with complex internal geometries (cold plates, radiators, and RF waveguides) are produced as brazed assemblies. These complex assemblies pose many manufacturing issues that typically lead to a low first-pass yield. As another option, UAM can be used to 3D print all grades of aluminum and Fig. 2...
Journal Articles
AM&P Technical Articles (2019) 177 (6): 18–22.
Published: 01 September 2019
... Radiograph of water header braze quality showing porosity, voids, and lack of bonding. Fig. 8 Radiograph showing cracked strands in copper conductors. Fig. 9 Radiograph showing cracks in water passages. can be manipulated to show porosity, voids, discontinuities, and operational damage, as well...
Journal Articles
AM&P Technical Articles (2021) 179 (6): 19–20.
Published: 01 September 2021
... blasting process which happens References 1. Welding, Brazing and Soldering, Vol 6, ASM Handbook, ASM International, 1993. 2. Surface Engineering, Vol 5, ASM Handbook, ASM International, 1994. 3. Materials Characterization, Vol 10, ASM Handbook, ASM International, 2019. ...
Journal Articles
AM&P Technical Articles (2023) 181 (1): 36–37.
Published: 01 January 2023
...@lejones.com. References 1. Welding, Brazing and Soldering, Vol. 6, ASM Handbook, ASM International, 1993. 2. Surface Engineering, Vol. 5, ASM Handbook, ASM International, 1994. 3. Materials Characterization, Vol. 10, ASM Handbook, ASM International, 2019. ...
Journal Articles
AM&P Technical Articles (2015) 173 (10): 63–65.
Published: 01 November 2015
... processes including annealing, brazing, and sintering. This article provides an overview of Hydroprime, a unique steam methane reformer that uses an integrated heat recovery system to reduce the cost and improve the reliability of hydrogen gas supply. Fig. 1 Gas atmospheres are used in the production...
Journal Articles
AM&P Technical Articles (2017) 175 (2): 59–61.
Published: 01 February 2017
... corrosion resistance everywhere else. Being able to synthesize substrates and structures from multiple materials would have a far reaching effect, offering a single new approach to many processes such as brazing and thermal spray. Instead of joining complex assemblies made of different thicknesses of cast...
Journal Articles
AM&P Technical Articles (2020) 178 (7): 19–21.
Published: 01 October 2020
... to machine. In this case, 3D printing was a logical alternative choice, providing design freedom and avoiding welding and brazing of separate parts (Fig. 1b). Surface finish directly out of the advanced AM system was also exceptionally high, reducing post-processing steps. Ti-6Al-4V KW Micro Power...