Abstract
This article describes Shear-Assisted Processing and Extrusion (ShAPE), an emerging extrusion technology being developed at the Pacific Northwest National Laboratory. One application of the ShAPE process is recycling post-consumer scrap without adding primary aluminum, which reduces embodied energy and carbon output. Scientists at PNNL won an R&D 100 Award in 2020 for their work in developing the ShAPE process.