Alloy developers worldwide have struggled to create creep-resistant alumina-forming, iron-based austenitic stainless steels for use as high-temperature structural alloys, but with limited success in balancing alloy cost, oxidation, and creep resistance. This article describes the research and development of a novel cast alumina-forming austenitic stainless steel. This work won the prestigious Engineering Materials Achievement Award presented at IMAT 2023 in Detroit.