Abstract
A mixed-reality application called HoloMicroscope helps microscopists make decisions and analyze data efficiently while using transmission electron microscopes. In the context of materials research, using mixed reality augments a user’s interaction by allowing them to see a TEM column and its control panels, while also interacting with three-dimensional holograms that are projected into their field of view. Introduction of mixed reality into a data-intensive research workflow could help accelerate scientific discovery. This article provides background about technology and a case study in its use.