Abstract
Additive manufacturing techniques give the mining industry a chance to revolutionize the conceptualization, prototyping, and production of mining tools, including using WC-Fe, Ni-based matrix coatings that display exceptional properties. The article includes a case study involving the successful utilization of WC-NiCrBSi mixed powder as a protective coating on AISI 9310 steel components to enhance wear resistance and durability for mining tool applications.