Integral quenching (IQ) is a widely adopted heat treatment technique known for its efficient and rapid quenching capabilities. Vertical vacuum IQ furnaces give heat treaters a larger working zone for efficient and rapid quenching. This article describes the elements of a vacuum IQ furnace line and describes its operational workflow and process control.