The July and September issues of the Journal of Materials Engineering and Performance (JMEP) were special issues focused on additive manufacturing. The issues were guest edited by William E. Frazier, FASM, Pilgrim Consulting LLC and editor of JMEP; Rick Russell, NASA; Yan Lu, NIST; Brandon D. Ribic, America Makes; and Caroline Vail, NSWC Carderock. The highlighted articles described in this article were selected by Dr. Frazier to showcase the varied topics covered in the special issues.