This entry won the prestigious Jacquet-Lucas Award for Best in Show in the 2020 International Metallographic Contest. In the research discussed in this article, light microscopy was applied to a Co28Cr6Mo alloy for a biomedical application processed by laser bed powder fusion (LPBF) additive manufacturing.