A joint Canadian venture launches a new facility with an innovative hybrid approach to cold spray additive manufacturing. The technology platform combines multiple manufacturing steps in a single cold spray additive manufacturing (CSAM) unit, incorporating surface preparation, cold spray forming and buildup, local laser-based thermal treatment, and in-situ sequential robotic machining and semi-finishing.