Abstract
This article describes a procedure for optimizing the annealed microstructure of a high Al KAB steel. The main focus is directed toward characterization of microstructural development during annealing of different phases in a nanostructured bainitic steel using high resolution transmission electron microscopy (HRTEM). This entry won the prestigious 2019 Jacquet-Lucas Award for Excellence in Metallography at the International Metallographic Contest held in Portland, Oregon, October 2019.