Characterizing ice and snow is important not only for building accurate climate models, but also for activities such as relating the mechanical properties of sea ice to its microstructure so that the interaction of ice with ships and structures can be better understood. This article describes the microstructural characterization of ice. Many microstructural characterization techniques that can be applied to other materials also can be used to examine ice.