Field assisted sintering technology (FAST) enables hybrid components for aerospace to be designed with reduced weight and without sacrificing performance. FAST can be used to produce metal, ceramic, and composite components with tailored properties via a powder metallurgy approach. In many cases, it is a one-step, cost-effective manufacturing process for production of net-shape components.