Abstract
High-speed, high-fidelity techniques used to analyze texture and dislocation content enable greater understanding of the influence of texture on deformation of titanium alloys than previously possible. This article describes a study in which specimens were examined using graphical slip band analysis to understand the influence of microstructure, alloy content, and loading orientation on the surface deformation response of titanium.