Abstract
An ultrafast, efficient industrial-scale boriding process can drastically reduce costs, increase productivity, and improve the performance and reliability of a variety of machine parts. This article describes a novel, environmentally friendly technology that enables treating thousands of industrial components in one batch, without creating solid or liquid waste and gaseous emissions.