Modeling shows that achieving required gear performance in a reduced gear size is possible by changing the steel grade and heat treatment parameters during the design stage. This article describes work in which virtual computer models using DANTE software are applied to help achieve gear size reduction by including steel grade hardenability and heat treatment parameters in the design process.