Abstract
Emissivity is a term used to define the ability of a surface to emit and absorb radiation. At any given temperature, the emissivity of a body (or surface) equals its absorptivity. Development work on a vacuum carburizing process revealed the need to better understand the effect of workload surface emissivity and the proper use of dummy thermocouple test blocks. This article reports on the findings from this research effort.